bioRxivBioengineering
Multiscale Multimodal Characterization and Simulation of Structural Alterations in Failed Bioprosthetic Heart Valves
E. Tsolaki, P. Corso, R. Zboray, J. Avaro, C. Appel, M. Liebi, S. Bertazzo, P. P. Heinisch, T. Carrel, D. Obrist, I. K. Herrmann
Abstract
Calcific degeneration is the most frequent type of heart valve failure, with rising incidence due to the ageing population. The gold standard treatment to date is valve replacement. Unfortunately, calcification oftentimes re-occurs in bioprosthetic substitutes, with the governing processes remaining poorly understood. Here, we present a multiscale, multimodal analysis of disturbances and extensive mineralisation of the collagen network in failed bioprosthetic bovine pericardium valve explants with full histoanatomical context. In addition to highly abundant mineralized collagen fibres and fibrils, calcified micron-sized particles previously discovered in native valves were also prevalent on the aortic as well as the ventricular surface of bioprosthetic valves. The two mineral types (fibers and particles) were detectable even in early-stage mineralisation, prior to any macroscopic calcification. Based on multiscale multimodal characterisation and high-fidelity simulations, we demonstrate that mineral occurrence coincides with regions exposed to high haemodynamic and biomechanical indicators. These insights obtained by multiscale analysis of failed bioprosthetic valves may serve as groundwork for the evidence-based development of more durable alternatives. Graphical Abstract O_FIG O_LINKSMALLFIG WIDTH=200 HEIGHT=176 SRC="FIGDIR/small/529530v1_ufig1.gif" ALT="Figure 1"> View larger version (57K): org.highwire.dtl.DTLVardef@c7e0b5org.highwire.dtl.DTLVardef@71bdbdorg.highwire.dtl.DTLVardef@15fdc23org.highwire.dtl.DTLVardef@6dbd1c_HPS_FORMAT_FIGEXP M_FIG C_FIG
Reproducibility ledger
Nobody has reported trying to reproduce this paper yet. Did you replicate an experiment or run the code? Your report saves the next lab a week.
Sign in to file a reproducibility report.
Related papers
- Collagen fibre-mediated mechanical damage increases calcification of bovine pericardium for use in bioprosthetic heart valves
A. Whelan, E. Williams, … C. Lally·bioRxiv·Oct 21, 2020
- Glycation and Serum Albumin Infiltration Contribute to the Structural Degeneration of Bioprosthetic Heart Valves
A. Frasca, Y. Xue, … G. Ferrari·bioRxiv·Feb 14, 2020
- Hydrogel-Polyurethane Fiber Composites With Enhanced Microarchitectural Control For Heart Valve Replacement
A. Robinson, A. Nkansah, … E. Cosgriff-Hernandez·bioRxiv·Sep 29, 2023
- In-vivo subdermal implant in the alpha-Gal knockout mice model for the assessment of bioprosthetic heart valve calcification rate before and after a polyphenols-based treatment
- Deterioration of Glutaraldehyde Crosslinked Heterograft Biomaterials due to Advanced Glycation End Product Formation and Serum Albumin Infiltration
C. A. Rock, S. Keeney, … R. J. Levy·bioRxiv·May 28, 2020
- Combined Raman Microscopy and Transmission Electron Microscopy shows the co-existence of whitlockite crystals and carbonated hydroxyapatite-mineralized collagen fibrils in human calcified aortic valves
Robin H.M. van der Meijden, Carolien Kuster, … Anat Akiva·bioRxiv·Mar 3, 2025